| Curing | |
|
Work life at 23°C |
3 minutes (2g) |
|
Curing Time @ 23°C vs. Hardness |
25D after 5 minutes 50D after 30 minutes 70D after 60 minutes |
| Properties before curing | |
| Mixed viscosity | 10 ÷ 15 Pa·s |
| Surface tension | 42 - 44 mN/m |
| Optimum properties (cured for 60' at 23°C) | |
|
Lap shear (Al/Al) |
8 MPa |
| Density | 1.20 |
| Hardness | 70D |
|
Thermal expansion |
55 x 10-6 cm/cm/°C |
| Operating temperature |
-60°C to +125°C |